So just to be clear, is Vette Panel Adhesive the preferred choice on the roof to quarter seam if lead is not used and you don't make a metal filler strip?
if your going to use filler then vpa is the better choice . DO NOT use any of that worthless duraglass or anything else made by dynatron bondo. fiberglass fillers are NOT water proof or superior to anything else.
Thanks guys. I was thinking of making metal filler strips but was also thinking IF the weld seam got a little too thick it would show some ghosting also.
Kent White ( The Tin Man) simplifies and makes lead work so simple in this DVD that anyone can do high quality work without fear. He also explains about a homemade flux that is more versatile, safer, and easier that any I have seen. http://www.tinmantech.com/html/vid_art_science_autobody.php