  1. V

    Glazing putty over 2k high build

    I'm working on a hood I have my filler as base then epoxy then 2k high build now I am glazing lows in my hood, what I am finding out is I am having to use alot more glazing putty than I intended on to get the hood straight, I am using pro glaze which has in the material sheet that it can be used...
  2. B

    poor adhesion spraying base next day

    Hi Guys, I sprayed some epoxy as a sealer, then the next day sprayed nason base the next day. This was the inside of some doors. About a month later I taped the inside of the doors off to not get overspray on them, but pulling the tape up pulled the clear and base right off of the epoxy. Is...