[/URL][/IMG] I've used SPI epoxy and Turbo primer. I am wondering about paint adhesion. The hood is wet sanded in 600 grit and already has a glass like appearance. Is the single stage paint going to stick with no problems? I am just a little concerned as it's been awhile since I have painted. I am trying to insert a picture. The picture was taken while wet. Thanks
600 grit is what I use all the time.
The wet look shows the water is sheeting rather than beading up and gives you an indicator of how the panel will look when buffed.
I forgot to mention also that I have noticed a very faint line in the primer when the hood is wet. Only visible when wet. A small dent in a couple spots. Not noticeable until wet. Can I simply re-spray some turbo primer over these areas to fill or do I need to use filler? Thanks
For filler you should scratch with 80 grit which should remove most of your primer.
If you see a line now, you will see a line later. If you see dents now, you will see dents later. Shoot more turbo and use a guide coat.