I can’t dip the car. I’m too far along w the restoration. I didn’t know about the pits bc years ago I coated the entire car in Fertan thinking it would protect the metal while I did the pans. The pits might have been there before bc the entire car had oxidation from when the PO sanded off the paint and then let it sit for 20+ years in his garage unprotected.Dip it or blast it.
I have not tried 36 grit yet. I have tried 80 with no success. I was worried that the 36 would remove too much metal thickness.Have you tried 36 and 80 grit on a DA? Or even something like an 8” mud hog. I don’t see how you can use ospho etc on a whole car.
Dipping might be an option but not sure if there are any dippers on Mars…![]()
How long did you leave the Opsho on? Before you go to aggressive sanding I would make sure you've tried leaving the acid on for a few hours and while it's wet scrubbing with a coarse scuff pad (I use the Duragold gold color - it's 150grit). Sometimes it takes a while for the cocktail to get into the small pits. I find another thing that helps lift out small rust pits is cleaning while doing acid work. I'll grab a new microfiber (why I keep cheap ones on hand) and wet it with distilled water and wipe the surface down. It helps lift any gunk off the surface the process is creating and gives the next application more bite...then more Ospho and you'll see the surface get brighter and cleaner. Sounds labor intensive but it's quick and not very wasteful, I'll keep empty dip cans for filling with acid and dipping my scuff pad in...can use this amount for the whole roof of a car.I need help with how to handle all the 1000’s of tiny pits in my sheet metal. I tried Ospho but it didn’t seem to touch the pits. I tried 3M Scotch-bright Rolocs, a surface conditioner tool etc but they remain. Advise is much appreciated. I am a hobbyist and this my Porsche 356 that sat unpainted but indoors for many years. The unprotected surface developed tiny rust pits all over it. I am not planning on painting the car right now. I’m going for a bare metal finish w something like Sharkhide, but I know I need to stop the rust first.
I have blasted before and of course this is an option, though a very messy one. Dipping is absolutely out of the question. The car is way to "assembled" for this option. The Ospho I have is very old, does it have a shelf life? Additionally, as suggested by Airheated, I have not left the Ospho on the car for a long period bc I am an impatient person. I will by some new material and be more patient. I agree, that sanding with 36 will be too aggressive as that is what I use for welding grinds.Every square inch of the car is pitted. I can’t imagine trying to fix that with ospho. The magnitude of the effort needed is huge….
Blasting all that is almost certain to distort the metal.
Maybe it’s time to back up, undo some stuff and get it dipped.
I disagree with that assessment.Every square inch of the car is pitted. I can’t imagine trying to fix that with ospho. The magnitude of the effort needed is huge….
Blasting all that is almost certain to distort the metal.
Maybe it’s time to back up, undo some stuff and get it dipped.
Well then I guess we have to agree to disagree. Metal distortion with blasting has nothing to do with heat. It is the peening action of the media hitting the panel that generates distortion. Yes hitting it an angle helps because it reduces the impact force. It’s just not as effective in deep pits when you hit it at an angle.I disagree with that assessment.
If you keep the air pressure down and hold the tip at a slight angle to the surface, it generates next to no heat at all. Personally, I have never had any metal warp when media blasting.
I have a 20 gallon blasting pot that I use for anything that can't fit in the blasting cabinet.
I agree 100%por15 says you can smear it right over all of that.
its a joke.
Glad I found this forum. I'm on one for Oldsmobiles a lot of them use por 15, I probably would have too.