New poster here. I blast and refinish antique and vintage metal patio furniture. Been using U-Tech epoxy then single stage, but recently tried SPI epoxy and like it. Got a few fisheyes and Barry suggested prepping with 700 waterborn w&g remover. My dilemma is the fine texture of my blast profile causes any wiping towels or rags to leave enough fiber "fur" to show up in the paint job. Tried using a red Scotchbrite instead of blue shop towels and fibers still present. Even after blowing off with a leaf blower. So here's my question:
If I hang the parts (after blasting) and douse them with enough 700 to drip off, can I avoid the whole wipe down process and still have good surface prep? I would still hit them with the leaf blower after dripping stopped.
Thanks,
Jeff
If I hang the parts (after blasting) and douse them with enough 700 to drip off, can I avoid the whole wipe down process and still have good surface prep? I would still hit them with the leaf blower after dripping stopped.